WEKO3
アイテム
{"_buckets": {"deposit": "6de4a584-8729-4621-9df2-f22de3c8bd04"}, "_deposit": {"created_by": 3, "id": "3606", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "3606"}, "status": "published"}, "_oai": {"id": "oai:toyama.repo.nii.ac.jp:00003606", "sets": ["567"]}, "author_link": ["54076", "54073", "54074", "54075", "54077", "54072"], "item_3_alternative_title_19": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "On the Electro-deposition of Metallic Selenium (the 2nd Report) : Effects of Nitrogen Containing Cyclic Compounds and Organic Colloids"}]}, "item_3_biblio_info_7": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1956-02-29", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "1/2", "bibliographicPageEnd": "67", "bibliographicPageStart": "62", "bibliographicVolumeNumber": "7", "bibliographic_titles": [{"bibliographic_title": "富山大学工学部紀要"}]}]}, "item_3_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "The effects of nitrogen containing cyclic compounds and organic colloids for the electro-deposition of Se from dilute sulphuric and bath were investigated. The results are as follows: -- \n(1) Addition of pyridine and quinoline fairly increases the metallic Se content in deposit, but their excess precipitate colloidal red Se and pollute the plating bath. \n(2) Gelatin, dextrin, molasses and glucose have no effect for the increment of metallic Se in deposit, and moreover make the deposite flaky. \n(3) Adherent state of deposit is something improved by the composite addition of pyridine and glucose.", "subitem_description_type": "Abstract"}, {"subitem_description": "前報に於ては亜セレン酸の酸性溶液から金属セレン電着について種々検討し,セレンの電着状態,電流効率と種々の電解条件との関連について実験した結果を報告した。\n即ち著者等が行った実験の範囲ではアルミニウム及び白金陰極に対して誕セレン酸濃度4~6m/L,硫酸0.2~0.4n,電流密度2~4A/d㎡,浴温90℃で暗灰色の可成良好なセレンの電着を得た。\n但し顕微鏡で観察すると金属セレンの結晶核が散在する程度で実際にはもっと金属化せしめる必要がある。\nそこで著者等は良好な状態の金属セレンを電着せしめるために,添加剤を用いてみた。\nSaundersによれば環中に窒素を有する環状化合物例えばピリヂン,キノリン,ピペリヂン等と無定形セレンを混んじて加熱するとセレンは金属セレンに変化すると言う。\nSaundersの実験は乾式の状態で行われたもので電着のような水溶液の状態では同じ作用があるかどうか疑問であるが,とにかく添加剤としてピリヂン及びキノリンを選んで電着浴に微量添加し電着実験を行ってみた。\nまた平滑な電着物を得るための添加剤として膠,ゼラチン等のコロイド物質は銅,錫,亜鉛等のメッキに実用されているがセレンの電着に於ても同じ作用があるかどうかは興味ある問題である。\nそこでゼラチン,デキストリン,糖密,葡萄糖を添加剤として選んでセレン電着に於ける影響を調べてみた。\n本報に於てはこれらの結果の要点を報告する。", "subitem_description_type": "Abstract"}]}, "item_3_description_40": {"attribute_name": "資源タイプ(DSpace)", "attribute_value_mlt": [{"subitem_description": "Article", "subitem_description_type": "Other"}]}, "item_3_description_6": {"attribute_name": "引用", "attribute_value_mlt": [{"subitem_description": "富山大学工学部紀要,7(1/2), Page 62-67", "subitem_description_type": "Other"}]}, "item_3_full_name_3": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "54075", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "YASUKAWA, Saburo"}]}, {"nameIdentifiers": [{"nameIdentifier": "54076", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "IZAKI, Tosio"}]}, {"nameIdentifiers": [{"nameIdentifier": "54077", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "ISINO, Siro"}]}]}, "item_3_identifier_registration": {"attribute_name": "ID登録", "attribute_value_mlt": [{"subitem_identifier_reg_text": "10.15099/00003600", "subitem_identifier_reg_type": "JaLC"}]}, "item_3_publisher_33": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "富山大学工学部"}]}, "item_3_source_id_10": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN00175872", "subitem_source_identifier_type": "NCID"}]}, "item_3_source_id_8": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "03871339", "subitem_source_identifier_type": "ISSN"}]}, "item_3_subject_22": {"attribute_name": "国立国会図書館分類", "attribute_value_mlt": [{"subitem_subject": "ZM2", "subitem_subject_scheme": "NDLC"}]}, "item_3_version_type_16": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "安川, 三郎"}], "nameIdentifiers": [{"nameIdentifier": "54072", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "位﨑, 敏男"}], "nameIdentifiers": [{"nameIdentifier": "54073", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "石野, 史郎"}], "nameIdentifiers": [{"nameIdentifier": "54074", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2016-02-16"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "Kokiyo_7_01_Page062to067.pdf", "filesize": [{"value": "13.7 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 13700000.0, "url": {"label": "Kokiyo_7_01_Page062to067.pdf", "url": "https://toyama.repo.nii.ac.jp/record/3606/files/Kokiyo_7_01_Page062to067.pdf"}, "version_id": "a8e021b8-b4e7-45a0-bc0c-3446dc96df6c"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "セレン", "subitem_subject_scheme": "Other"}, {"subitem_subject": "電着", "subitem_subject_scheme": "Other"}, {"subitem_subject": "ピリヂン系化合物", "subitem_subject_scheme": "Other"}, {"subitem_subject": "コロイド物質添加", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "departmental bulletin paper", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "セレンの電着に関する研究(第2報) : 稀硫酸浴(その2) : ビリヂン系化合物及びコロイド物質添加の影響について", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "セレンの電着に関する研究(第2報) : 稀硫酸浴(その2) : ビリヂン系化合物及びコロイド物質添加の影響について"}]}, "item_type_id": "3", "owner": "3", "path": ["567"], "permalink_uri": "https://doi.org/10.15099/00003600", "pubdate": {"attribute_name": "公開日", "attribute_value": "2012-08-21"}, "publish_date": "2012-08-21", "publish_status": "0", "recid": "3606", "relation": {}, "relation_version_is_last": true, "title": ["セレンの電着に関する研究(第2報) : 稀硫酸浴(その2) : ビリヂン系化合物及びコロイド物質添加の影響について"], "weko_shared_id": -1}
セレンの電着に関する研究(第2報) : 稀硫酸浴(その2) : ビリヂン系化合物及びコロイド物質添加の影響について
https://doi.org/10.15099/00003600
https://doi.org/10.15099/00003600ea5df2d4-344e-472e-a6df-9de1924a3a60
名前 / ファイル | ライセンス | アクション |
---|---|---|
Kokiyo_7_01_Page062to067.pdf (13.7 MB)
|
|
Item type | 紀要論文 / Departmental Bulletin Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-08-21 | |||||
タイトル | ||||||
タイトル | セレンの電着に関する研究(第2報) : 稀硫酸浴(その2) : ビリヂン系化合物及びコロイド物質添加の影響について | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | セレン | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | 電着 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | ピリヂン系化合物 | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | コロイド物質添加 | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | departmental bulletin paper | |||||
ID登録 | ||||||
ID登録 | 10.15099/00003600 | |||||
ID登録タイプ | JaLC | |||||
著者 |
安川, 三郎
× 安川, 三郎× 位﨑, 敏男× 石野, 史郎 |
|||||
著者別名 | ||||||
姓名 | YASUKAWA, Saburo | |||||
著者別名 | ||||||
姓名 | IZAKI, Tosio | |||||
著者別名 | ||||||
姓名 | ISINO, Siro | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | On the Electro-deposition of Metallic Selenium (the 2nd Report) : Effects of Nitrogen Containing Cyclic Compounds and Organic Colloids | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | The effects of nitrogen containing cyclic compounds and organic colloids for the electro-deposition of Se from dilute sulphuric and bath were investigated. The results are as follows: -- (1) Addition of pyridine and quinoline fairly increases the metallic Se content in deposit, but their excess precipitate colloidal red Se and pollute the plating bath. (2) Gelatin, dextrin, molasses and glucose have no effect for the increment of metallic Se in deposit, and moreover make the deposite flaky. (3) Adherent state of deposit is something improved by the composite addition of pyridine and glucose. |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | 前報に於ては亜セレン酸の酸性溶液から金属セレン電着について種々検討し,セレンの電着状態,電流効率と種々の電解条件との関連について実験した結果を報告した。 即ち著者等が行った実験の範囲ではアルミニウム及び白金陰極に対して誕セレン酸濃度4~6m/L,硫酸0.2~0.4n,電流密度2~4A/d㎡,浴温90℃で暗灰色の可成良好なセレンの電着を得た。 但し顕微鏡で観察すると金属セレンの結晶核が散在する程度で実際にはもっと金属化せしめる必要がある。 そこで著者等は良好な状態の金属セレンを電着せしめるために,添加剤を用いてみた。 Saundersによれば環中に窒素を有する環状化合物例えばピリヂン,キノリン,ピペリヂン等と無定形セレンを混んじて加熱するとセレンは金属セレンに変化すると言う。 Saundersの実験は乾式の状態で行われたもので電着のような水溶液の状態では同じ作用があるかどうか疑問であるが,とにかく添加剤としてピリヂン及びキノリンを選んで電着浴に微量添加し電着実験を行ってみた。 また平滑な電着物を得るための添加剤として膠,ゼラチン等のコロイド物質は銅,錫,亜鉛等のメッキに実用されているがセレンの電着に於ても同じ作用があるかどうかは興味ある問題である。 そこでゼラチン,デキストリン,糖密,葡萄糖を添加剤として選んでセレン電着に於ける影響を調べてみた。 本報に於てはこれらの結果の要点を報告する。 |
|||||
引用 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 富山大学工学部紀要,7(1/2), Page 62-67 | |||||
書誌情報 |
富山大学工学部紀要 巻 7, 号 1/2, p. 62-67, 発行日 1956-02-29 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 03871339 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN00175872 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
国立国会図書館分類 | ||||||
主題Scheme | NDLC | |||||
主題 | ZM2 | |||||
出版者 | ||||||
出版者 | 富山大学工学部 | |||||
資源タイプ(DSpace) | ||||||
内容記述タイプ | Other | |||||
内容記述 | Article |